E41-537 · Bearing Selection · Copper Bar Damaging the Bearing End Face During Installation · ★★★
When installing the bearing the operator hammered the end face of the inner ring with a copper bar (pure copper). The copper bar deformed (crushed) during hammering, the blows were uneven and dents were produced on the inner ring end face.
The operator used a Φ20mm pure copper bar (hardness HB35) against the end face of the inner ring and struck the bar with a hand hammer. The hardness of the copper bar is far below that of bearing steel (HRC62 ≈ HB700), so under the hammering force (about 5000N) the end of the bar was crushed by about 0.2mm and the contact area against the inner ring end face changed from the design value (the full end face) to local contact (about 10% of the area). The compressive stress in the local contact zone is σ_c=F/A_actual=5000/(0.1×π×0.015×0.002)≈530MPa (A_actual ≈ 10% of the inner ring end face area = 0.1×π×30×2 ≈ 19mm²). At 530MPa local stress the inner ring end face develops dents (depth about 0.005mm). The dents cause end-face runout so that the inner ring tilts after installation, producing stress concentration in the raceway. In severe cases the raised material at the edge of the dents prevents the bearing from being pushed fully into place.
1) Bearing installation should preferably use dedicated pressing tools (a press or a puller);
2) If a bar must be used, use a beryllium copper bar (hardness HB100, resistant to crushing);
3) Machine the end of the bar into an annular face matching the inner ring end face (to increase the contact area);
4) Hammering the bearing end face directly with a hammer is strictly prohibited;
5) After installation, check that the bearing rotates freely (it should turn smoothly by hand).
FT_23_Bearing Selection Standards