E41-787 · Other Selection · Hydrostatic Test Cracking · ★★★★★
A pressure vessel (design pressure 1.0 MPa, Q345R plate, wall 8 mm) cracked during hydrostatic testing (test pressure 1.5 MPa).
GB 150 sets hydrostatic test pressure P_test = 1.25×P_design×[σ]/[σ]t = 1.25×1.0×189/170 = 1.39 MPa ([σ] = 189 MPa allowable stress at ambient, [σ]t = 170 MPa at design temperature). The actual test used P_test = 1.5 MPa > 1.39 MPa, 8% overpressure. Vessel hoop stress σ_θ = P×D/(2×t) = 1.5×1000/(2×8) = 93.75 MPa. Q345R yield σ_s = 345 MPa, S = 345/93.75 = 3.68, so it should not crack. Cracking was at the shell-to-head circumferential weld (leg height 6 mm); the weld was made without bevel (plate 8 mm should have a single-V bevel), penetration only 3 mm (incomplete fusion), so the effective wall at the unwelded-through spot is the leg height (6 mm), not the plate thickness (8 mm). Fillet weld shear strength is by leg: τ = F/(0.7×h×L) = P×D×L/(4×0.7×h×L) = 1.5×1000/(2.8×6) = 89.3 MPa (L = weld perimeter). Q345R weld allowable shear about 120 MPa, S = 120/89.3 = 1.34, weld margin below 1.5. The actual weld had defects (undercut 0.5 mm deep, porosity Φ1 mm at 5 mm pitch); stress concentration factor about 2.5 → local stress σ_peak = 89.3×2.5 = 223 MPa > 120 MPa → weld cracked.
① Recheck all parameters per correct selection specifications
② Confirm that operating loads, environment, and service life all meet design requirements
③ Select reliable brands and appropriate models
④ Verify installation and operating conditions
⑤ Perform periodic inspection and maintenance after commissioning
FT_Machine Design Handbook