E41-678 · Hydraulic Component Selection · Hydraulic Cylinder Internal Leakage · ★★★★
When the cylinder was holding pressure the pressure fell from 16 MPa to 8 MPa every 5 min, and the piston seal was worn.
In high-speed reciprocating motion the polyurethane seal heated up through friction to 90℃ (limit 80℃); once its strength dropped it was extruded into the clearance and damaged.
① Use a PTFE + bronze composite seal for high-speed cylinders
② Keep the seal clearance ≤0.2 mm
③ Machine the seal groove to standard