E41-895 · Seal Component Selection · Acid Pump Mechanical Seal · ★★★★
One 30% sulfuric acid pump mistakenly used a fluororubber ring (actually acid-resistant, but the selection sheet wrongly issued NBR); the NBR swelled and cracked, leaking acid and injuring someone.
First, NBR resists mineral oil but not strong acid; 30% sulfuric acid makes it swell >40% by volume and lose strength. Second, the swollen ring splits and acid escapes. Third, acid injured a person despite insurance. Root cause: wrong material issued / compatibility error.
① Select acid/alkali media by the compatibility table (sulfuric acid: FKM/FFKM/PTFE; NBR/EPDM prohibited depending on concentration)
② The selection sheet must state medium concentration and temperature
③ Verify received material matches the BOM
④ If medium is unknown, send samples for testing
⑤ Use FFKM/PTFE for strong corrosion
⑥ Do not issue material by experience alone
⑦ If acid leaks, check the material immediately
FT_Seal Spring Design