E42-214 · Fatigue Fracture · Vibrating Screen Exciter · ★★★
After 800h, bolt seat surface pit depth 0.4mm; connection loosens.
[Washer Indentation] Spring washer low hardness; under preload F=30kN seat pressure p=620MPa exceeds yield. [Fatigue Pit] Under alternating vibration, repeated plastic deformation of seat creates 0.4mm pit. [Design Omission] Spring washer misused to carry vibratory load; seat not hardened.
1. Switch to disc spring washer + flat washer combination.
2. Harden clamped-part seat surface to HRC40.
3. Set bolt preload F=45kN.
4. Add nylon lock nut for anti-loosening.
5. Add hardened washer Φ24 on seat.
6. Shipment connection inspection on vibration section.
7. Shift-point loosening inspection.
8. Quarterly preload recheck.
GB/T 93-1987