E42-514 · Casting Defects · Aluminum Alloy Gearbox · ★★
Housing blowholes φ3, leaking on oil-pressure test; scrap rate 6%; 4 parts scrapped per month
[Blowhole] High sand moisture and gas evolution; entrapped gas φ3.
[Process] Fast pouring, poor venting.
[Design Omission] Sand moisture not controlled, poor gating design; safety factor 1.3 (should be ≥2.0).
1) Control sand moisture to ≤4%;
2) Add vent channels;
3) Lower pouring speed;
4) Check blowholes per heat;
5) Limit wall thickness;
6) Pressurized casting;
7) Impregnation sealing;
8) Periodic pressure test.
GB/T 1173-2013