Inclusions in Crankshaft Casting

E42-515 · Casting Defects · Ductile Iron Crankshaft (QT700) · ★★

Problem Description

Slag inclusion at the journal 20mm long, fracture risk; scrap rate 5%; 3 parts scrapped per month

Root Cause

[Inclusion] Poor slag trapping in gating; slag enters the cavity 20mm long.
[Inoculation] Poor spheroidization, flake graphite present.
[Design Omission] No slag trapping, insufficient inoculation; safety factor 1.3 (should be ≥2.0).

Corrective Solution

1) Provide filter screen;
2) Fully inoculate;
3) Raise nodularity;
4) Check inclusions per heat;
5) Limit pouring head height;
6) Purify the molten iron;
7)NDE;
8) Periodic re-measurement.

Checklist

Reference

GB/T 1348-2009