Non-Uniform Quenching Cooling Causes Warping of Thin-Walled Parts

E42-016 · Heat Treatment Distortion & Cracking · Thin Gear (20CrMnTi) · ★★★

Problem Symptom

Flatness 0.15mm (allowable 0.05), which cannot be corrected in subsequent operations

Root Cause

[Non-Uniform Cooling] The cooling rate difference between the two sides of the thin wall is ΔT=180℃, giving a thermal stress σ_th=EαΔT=2.1e5×1.2e-5×180=450MPa.
[Warping Amount] Non-uniform phase transformation plus thermal stress gives a flatness error f=0.15mm, 3 times out of tolerance.
[Design Omission] Press quenching was not used and cooling was non-uniform, so the warping exceeded tolerance by 3 times.

Correct Solution

1) Use press quenching to restrain deformation;
2) Control the quench oil temperature at 60±5 for uniformity;
3) Add process bosses on the thin wall;
4) Use stepped quenching to reduce stress;
5) Add a straightening operation;
6) Inspect flatness 100% on a three-coordinate measuring machine;
7) Optimise the fixturing method;
8) Feed the heat treatment deformation data into the quenching process library.

Checklist

References

GB/T 16923 Normalising and Annealing of Steel Parts

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL