❌ Error Case Studies

📚 Technical Articles

Insufficient Induction Hardened Case Depth on the Crankshaft Main Journal Causes Early Surface Indentation

E42-068 · Heat Treatment Distortion & Cracking · Crankshaft 45 Steel · ★★

Problem Symptom

Hardened case 1.2mm (3mm required), early indentation and pitting

Root Cause

[Insufficient Case Depth] The high-frequency power was too low and the case depth is only 1.2mm, so plastic indentation occurs under contact stress.
[Indentation] The contact pressure exceeds the yield strength of the surface layer and pitting appears.
[Design Omission] The quenching power and time were not controlled and the case depth was not measured, so the part failed early.

Correct Solution

1) Adjust the high-frequency power and time to give a case depth ≥3mm;
2) Measure the case depth for every batch;
3) Control the surface hardness to HRC55-60;
4) Temper after quenching;
5) Use induction hardening of the fillet to avoid fracture;
6) Perform magnetic-particle inspection;
7) Check the hardness gradient;
8) Make the case depth a dedicated inspection item.

Checklist

References

JB/T 6727-2001 Internal Combustion Engine Crankshafts — Technical Conditions