Surface Spalling on Induction-Hardened Gear

E42-341 · Heat Treatment Distortion and Cracking · Induction-Hardened Gear · ★★

Problem Description

The induction-hardened gear (40Cr) has surface spalling and pitting; 3 parts scrapped per month

Root Cause

[Hardness Gradient] Large hardness difference between hardened layer and core; transition zone brittle.
[Spalling] Hardened layer depth 0.8mm uneven; surface layer spalls.
[Design Omission] Frequency not controlled, case depth uneven; safety factor only 1.2.

Corrective Solution

1) Control hardened case depth to 1.0-1.5mm;
2) Variable-frequency uniform heating;
3) Post-quench temper stress relief;
4) Smooth the transition zone;
5) Measure case depth each batch;
6) Hardness gradient inspection;
7) Limit working contact stress;
8) Periodic inspection.

Checklist

Reference

GB/T 16924-2008