Tooth Corner Chipping on Carburized Gear

E42-342 · Heat Treatment Distortion and Cracking · Carburized Gear · ★★

Problem Description

The carburized gear (20CrMnTi) has tooth-corner chipping and broken teeth; 2 parts scrapped per month

Root Cause

[High Carbon Brittle] Surface carbon concentration 1.2% too high; coarse brittle martensite.
[Corner Chipping] Stress concentration at the tooth corner causes chipping.
[Design Omission] Carbon potential not controlled, no slow cooling; safety factor only 1.2.

Corrective Solution

1) Control carbon potential to 0.8-1.0%;
2) Tooth corner fillet R≥0.5mm;
3) Slow cool to reduce cracking;
4) Double tempering;
5) Measure carbon concentration each batch;
6) Metallographic examination;
7) Limit working load;
8) Periodic inspection.

Checklist

Reference

GB/T 8539-2008

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »