E42-478 · Heat Treatment Distortion and Cracking · Large Gear · ★★
The large gear (φ1500) warps 0.25mm in flatness after quench-and-temper, with meshing noise; 1 part scrapped per month
[Warpage] Uneven cooling; thermal stress causes 0.25mm warpage.
[Abnormal noise] Mesh offset.
[Design Omission] No press hardening, no aging; safety factor 1.4 (should be ≥2.0).
1) Press-quench to limit distortion;
2) Uniform quench-oil temperature 60±5℃;
3) Age after quench-and-temper;
4) Finish-grind the flat face;
5) Measure flatness each part;
6) Limit cooling rate;
7) Add process bosses;
8) Periodic re-measurement.
GB/T 8539-2008