Quench Cracking of Tool Die

E42-479 · Heat Treatment Distortion and Cracking · Cold-Working Die · ★★

Problem Description

The cold-working die (Cr12MoV) has quench cracks 80mm long and is scrapped; 2 parts scrapped per month

Root Cause

[Quench Crack] Heated to 870℃ and fast-cooled; thermal stress + transformation stress cause cracking.
[Crack] Initiated at sharp corners.
[Design Omission] No pre-cooling, no grading; safety factor 1.2 (should be ≥2.0).

Corrective Solution

1) Martemper to reduce stress;
2) Pre-cool to 780℃;
3) Sharp-corner R≥3mm;
4) Thorough tempering;
5) NDE each piece;
6) Control heating rate;
7) Upgrade material toughness;
8) Periodic re-measurement.

Checklist

Reference

GB/T 1299-2014