Small Under-Head Fillet on High-Strength Bolt Causing Under-Head Fracture

E42-282 · Threaded Fastener Loosening · High-Strength Bolt · ★★

Problem Description

Grade 10.9 M20 bolts fracture at the under-head fillet, head separates from shank; 5 bolts fracture per month

Root Cause

[Small Fillet] Under-head fillet r=0.5mm (should be ≥1mm); per Kt=1+2√(h/r) gives Kt=2.5.
[Fracture] Preload tensile stress σ=700MPa exceeds the material fatigue limit; cracks initiate under the head and fracture.
[Design Omission] Fillet not controlled, no cold-heading transition; safety factor 1.2 (should be ≥2.0).

Corrective Solution

1) Under-head fillet ≥1mm;
2) Cold-headed forming transition;
3) Roll-thread strengthen the shank;
4) Control preload to 0.7σs;
5) Magnetic-particle inspection under head each batch;
6) Material re-verification (grade 10.9 certificate);
7) Torque-limiting wrench to prevent over-torquing;
8) Torque-method assembly.

Checklist

Reference

GB/T 3098.1-2010

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL