Sharp Corner of the Keyway Causes Fatigue Cracking of the Shaft

E42-022 · Stress Concentration · Gearbox Input Shaft · ★★★

Problem Symptom

Crack at the keyway end after 10 months of running, shaft broken

Root Cause

[Concentration Factor] The keyway end is a sharp right angle r=0 with Kt≈3.5, so a nominal stress of 110MPa becomes a local stress of 385MPa.
[Fatigue] 385MPa exceeds the corrected endurance limit of 200MPa, so a crack initiates at N=2e7 cycles, about 10 months.
[Design Omission] The keyway had no arc transition and no strengthening, so the shaft broke and production stopped.

Correct Solution

1) Add an R2 arc at the keyway end;
2) Provide a fillet transition at the shoulder;
3) Strengthen the fillet by roller burnishing;
4) Verify a fatigue life of ≥10 years;
5) Perform flaw detection;
6) Run a first-article bench test;
7) Quench and temper the material;
8) Include the keyway arc transition in shaft design review.

Checklist

References

GB/T 1095 Parallel Keys and Keyways