E42-124 · Stress Concentration · Planetary Reducer Planet Carrier · ★★
Fatigue cracks at the pin hole edges, the carrier body cracked
[Hole Edge Stress] The plain hole edges have right angles with no chamfer, giving Kt=2.3 under the alternating crushing of the pin.
[Fatigue] The hole edge stress exceeds σ-1, and the crack origin propagates.
[Design Omission] The hole mouth was neither chamfered C1 nor dimpled and the stress was not checked.
1) Chamfer the pin hole mouth C1 or dimple it;
2) Check the hole edge stress by finite element;
3) Finish the hole wall by fine reaming to reduce roughness;
4) Surface harden the pin;
5) Perform magnetic-particle inspection every 2500 running hours;
6) Keep the assembly coaxiality ≤0.02;
7) Measure the actual load spectrum;
8) Include the hole edge stress in the review.
GB/T 1804 General Tolerances