E42-173 · Stress Concentration · Ductile-Iron Bracket R3 · ★★
Bracket corner cracks; fracture shows a sharp-corner origin.
[Small Fillet] Corner R=3mm; theoretical stress concentration α=2.5. [Cracking] Operating tensile stress 80MPa amplified to 200MPa cracks. [Design Omission] R≥0.1t not taken, no fillet FEA; cracking rate 9%.
1. Take corner fillet R≥0.1t.
2. Smooth transition at fillet, no sharp corners.
3. Run fillet FEA stress check.
4. Polish fillet surface Ra3.2.
5. Add taper at thick-thin transition.
6. Casting fillet matches machining.
7. Magnetic-particle inspection at crack-prone locations.
8. Static-load fracture verification on the first piece.
GB/T 1348-2019