Pitting Corrosion Perforates the Stainless Steel Casing

E42-030 · Corrosion Failures · Chemical Pump Casing (304) · ★★★

Problem Symptom

Pitting perforation and leakage in a chloride-containing medium

Root Cause

[Pitting Potential] In 304 stainless steel with Cl->200ppm the pitting potential Eb is exceeded.
[Perforation Rate] The pitting pit depth grows at 0.5mm per year, so a 6mm wall perforates in two years.
[Design Omission] The wrong material was selected (316L required) and chloride was not controlled, so perforation occurred.

Correct Solution

1) Change to 316L or duplex stainless steel;
2) Control the chloride content of the medium to ≤50ppm;
3) Apply passivation treatment;
4) Add 2mm of corrosion allowance to the wall;
5) Measure wall thickness online;
6) Open the casing for periodic inspection;
7) Provide material certificates;
8) Include a media corrosion assessment in pump casing material selection.

Checklist

References

GB/T 3280 Cold-Rolled Stainless Steel

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL