E42-130 · Corrosion Failures · Cooling Water Pump Impeller · ★★
Dense pitting on the inlet edge of the impeller, the flow drops by 20%
[Cavitation] The pressure at the impeller inlet falls below the vapour pressure so bubbles form, and their collapse causes pitting.
[Pitting] Repeated bubble collapse produces honeycomb pits on the metal surface and the flow falls.
[Design Omission] The NPSH margin was insufficient and the impeller material was not cavitation resistant.
1) Raise the available NPSH of the installation;
2) Change the impeller to a cavitation-resistant duplex stainless steel;
3) Add a flow straightener at the inlet to prevent vortices;
4) Reduce the speed to lower the inlet velocity;
5) Round the impeller inlet edge;
6) Re-test the flow performance;
7) Open the casing periodically to check for pitting;
8) Include cavitation in pump selection.
GB/T 3216 Rotary Power Pumps — Hydraulic Performance Acceptance