E42-180 · Corrosion Failure · 316L/Carbon Steel Composite Pipe · ★★★
Pitting in the weld heat-affected zone connected into patches, leaking.
[Galvanic + Crevice] Potential difference between 316L and carbon steel 0.2V, weld crevice formed an occluded cell. [Composite Corrosion] Pitting connected at the crevice, wall thinned and perforated. [Design Omission] No transition section and no filler isolation; leakage caused production shutdown.
1. Add a stainless steel transition section between 316L and carbon steel.
2. Isolate the weld with nickel-based filler metal.
3. Fill the crevice with adhesive for sealing.
4. Apply an anti-corrosion coating on the outer surface.
5. Select materials with potential difference ≤0.1V.
6. Periodic PT inspection of the weld.
7. Reduce Cl- concentration in the medium.
8. Leak monitoring alarm.
GB/T 5776-2005