Knowledge Base › Structural Design Error Case Study › Stainless Steel Pitting Perforation Caused by Crevice Plus Chloride Ions

Stainless Steel Pitting Perforation Caused by Crevice Plus Chloride Ions

E42-246 · Corrosion Failure · Coastal Cooling Water Pipe · ★★★

Problem Description

After 8 months of operation, pitting at the flange crevice perforated and leaked water.

Root Cause

[Crevice Chloride Accumulation] Liquid accumulated in the flange gasket crevice containing Cl-, oxygen concentration cell formed. [Pitting Perforation] Cl- destroyed the passive film, pitting pits 2mm deep penetrated the wall thickness. [Design Omission] No chloride-resistant steel, unsealed crevice, and no corrosion inhibition.

Corrective Solution

1. Change the pipe to chloride-resistant 316L.
2. Inject sealant into the flange crevice for sealing.
3. Add corrosion inhibitor to control Cl-<25ppm.
4. Use chloride-free rubber gaskets.
5. Measure wall thickness quarterly.
6. Provide cathodic protection.
7. Increase flow velocity to 1.5m/s to prevent accumulation.
8. Open and inspect for corrosion annually.

Checklist

Reference

GB/T 20878-2007