Knowledge Base › Structural Design Error Case Study › Exhaust Manifold Eroded by High-Temperature Oxidation

Exhaust Manifold Eroded by High-Temperature Oxidation

E42-249 · Corrosion Failure · Engine exhaust manifold · ★★★

Problem Description

After two years, the manifold wall thinned and locally burned through.

Root Cause

[High-temp oxidation] Exhaust gas at 750℃; oxide scale on ordinary cast iron spalled and thinned the wall. [Burn-through] Long-term oxidation reduced the wall from 5mm to 1mm and burned through. [Design Omission] No heat-resistant steel, insufficient wall thickness margin.

Corrective Solution

1.Change manifold to heat-resistant cast steel R25.
2.Increase wall thickness from 5mm to 7mm.
3.Apply external high-temp anti-oxidation coating.
4.Use heat shield to lower wall temperature.
5.Measure thickness every 2 years.
6.Limit exhaust temperature to ≤800℃.
7.Casting free of blowholes.
8.Check fatigue life.

Checklist

Reference

GB/T 8492-2014

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »