Knowledge Base › Structural Design Error Case Study › Delayed Embrittlement Fracture of Plated High-Strength Bolt by Hydrogen Embrittlement

Delayed Embrittlement Fracture of Plated High-Strength Bolt by Hydrogen Embrittlement

E42-297 · Corrosion Failure · Electroplated high-strength bolt · ★★★

Problem Description

Grade 10.9 plated bolt fractured delayed by embrittlement 48h after plating; 3 bolts per month fractured

Root Cause

[Hydrogen embrittlement] Hydrogen absorbed during plating without baking; hydrogen content [H]=6ppm (should be ≤2), causing hydrogen-induced delayed embrittlement.
[Delayed fracture] Embrittlement fracture at 48h; fracture surface intergranular.
[Design Omission] No baking, strength grade 10.9 sensitive to hydrogen embrittlement; safety factor 1.3 (should be ≥2.0).

Corrective Solution

1) Bake at 200℃ for 4h after plating to remove hydrogen;
2) Lower strength grade to 8.8;
3) Change to electroless plating;
4) Test hydrogen content per batch to ≤2ppm;
5) Re-test material;
6) Replace with spares;
7) Standardize baking process;
8) Replace at end of life.

Checklist

Reference

GB/T 5267.1-2002