Knowledge Base › Structural Design Error Case Study › Pitting Perforation of Seawater Cooler Tube Bundle

Pitting Perforation of Seawater Cooler Tube Bundle

E42-431 · Corrosion Failure · BR0.3 seawater cooler titanium tube · ★★★

Problem Description

BR0.3 seawater cooler (316L) tube bundle: 12 tubes pitted through after 2 years, tube plugging reduced heat transfer; repaired twice a year

Root Cause

[Pitting] Seawater Cl⁻ (19000ppm) enriched, passive film locally broken, pitting rate 0.5mm/a. [Perforation] Tube wall 2mm thick, perforated in 2 years. [Design Omission] No Cl⁻-resistant material, no cathodic protection; safety factor 1.2 (should be ≥2.0).

Corrective Solution

1) Change tube material to titanium or duplex steel;
2) Add sacrificial anode protection;
3) Control flow velocity 1.5~2.5m/s;
4) Periodic cleaning;
5) Measure thickness quarterly;
6) Water quality monitoring;
7) Add corrosion inhibitor;
8) Replace tubes at end of life.

Checklist

Reference

GB/T 151-2014

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »