E42-440 · Corrosion Failure · FRP cooling tower support · ★★
FRP cooling tower steel support (humid): microbial corrosion, section thinned 30%, collapse risk; repaired twice a year
[Microbiological corrosion] Oxygen concentration under biofilm, corrosion rate 0.3mm/a. [Thinning] Section steel thins 0.3mm per year, instability. [Design Omission] No biocidal coating, insufficient corrosion protection; safety factor 1.3 (should be ≥2.0).
1) Change support to hot-dip galvanized section steel;
2) Add biocidal algaecide;
3) Thicken coating;
4) Measure thickness quarterly;
5) Ventilate and dehumidify;
6) Water treatment;
7) Limit load;
8) Replace at end of life.
GB/T 7190.1-2018