E42-475 · Corrosion Failure · Seawater pump impeller · ★★

Problem Description

Seawater pump (CD4MCu) impeller: pitting pits 2mm deep, efficiency dropped 15%; 1 unit replaced per month

Root Cause

[Pitting] High Cl- concentration, passive film broken, pitting pits 2mm deep.
[Pit] Stress concentration.
[Design Omission] No corrosion-resistant material, no cathodic protection; safety factor 1.3 (should be ≥2.0).

Corrective Solution

1) Change impeller to duplex steel 2205;
2) Add cathodic protection;
3)CoatingGuard;
4) Control flow velocity ≤3m/s;
5) Measure thickness quarterly;
6) Limit Cl-;
7) Polish surface;
8) Periodic re-measurement.

Checklist

Reference

GB/T 2100-2018