E42-529 · Corrosion Failure · Liquid ammonia storage tank · ★★★
Weld heat-affected zone SCC crack 40mm long, leaking; repaired once a year
[SCC] Tensile stress plus NH3, sensitized grain-boundary crack 40mm.
[Sensitization] Welding heat.
[Design Omission] No solution treatment, no stress relief; safety factor 1.2 (should be ≥2.0).
1) Post-weld solution treatment;
2) Stress-relief annealing;
3) Shot peening to introduce compressive stress;
4) Crack inspection quarterly;
5) Limit NH3 concentration;
6)Coating;
7) Control temperature;
8) Periodic NDE.
GB/T 150.1-2011