Wear-Corrosion of Pump Shaft

E42-530 · Corrosion Failure · Chemical process pump · ★★

Problem Description

Shaft φ50: medium scouring plus corrosion, diameter reduced 0.4mm per year, leaking; 2 shafts replaced per year

Root Cause

[Erosion] Flow velocity v=4m/s, solid-particle scouring plus corrosion reduces 0.4mm per year.
[Material] Not corrosion-resistant.
[Design Omission] No hardening, no liner; safety factor 1.3 (should be ≥2.0).

Corrective Solution

1) Hard-face weld on shaft surface;
2) Add bushing;
3) Lower flow velocity;
4) Diameter measurement monthly;
5) Limit particles;
6) Corrosion-resistant material;
7)Cathodic protection;
8) Periodic re-measurement.

Checklist

Reference

GB/T 5656-2008