Rough Interference Fit Surfaces Causing Assembly Adhesion and Scuffing

E42-185 · Fit and Interference Failure · Motor Rotor Shrink-Fit Shaft · ★★

Problem Description

After shrink-fitting, the rotor and shaft scuffed; hard to disassemble and surface scored.

Root Cause

[Roughness] Fit surface Ra3.2; asperities welded together under interference. [Adhesion] Disassembly scoring 0.2mm deep; fit failed. [Design Omission] Ra not controlled to ≤0.8, no molybdenum disulfide coating; rotor scrapped.

Corrective Solution

1. Control fit surface roughness to Ra≤0.8.
2. Apply molybdenum disulfide before shrink-fitting.
3. Take the median interference from calculation.
4. Heat uniformly to prevent local overheating.
5. Use special tooling for assembly.
6. Use a hydraulic puller for disassembly.
7. Prevent bumping of the surface.
8. Perform a torque transfer test after assembly.

Checklist

Reference

GB/T 5371-2004

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »