E42-190 · Structural Instability and Buckling · Dust duct Φ800×3 · ★★★
During hoisting compression, ductwork globally buckled, circumferential wrinkles wavelength ≈60mm, ovality out of tolerance 5%.
[Axial buckling] Thin-wall cylinder critical axial compression P_cr=2πEt²/(√3(1-ν²)) low, actual load exceeded. [Global instability] Shell circumferential wrinkle wavelength ≈1.7√(Rt). [Design Omission] Wall 3mm insufficient, no ring ribs; hoisting deformation.
1. Increase wall thickness to ≥5mm.
2. Add external circumferential stiffeners.
3. Check P_cr for axial buckling.
4. Add internal support during hoisting.
5. Control ovality ≤1%.
6. Upgrade material yield strength.
7. FE buckling analysis.
8. Factory collapse test.
GB 50018-2002