E42-147 · Residual Stress Distortion · Hydraulic Cylinder Piston Rod · ★★
The rod bends 0.08mm over the full length after deep-hole drilling
[Machining Residual Stress] Uneven plastic deformation of the surface layer during deep-hole drilling leaves residual stress, which bends the rod once released.
[Deformation] After material removal the stress redistributes and the rod bends by 0.08mm.
[Design Omission] Neither straightening nor ageing was applied.
1) Add a straightening operation after deep-hole drilling;
2) Apply stress-relief ageing;
3) Optimise the drilling parameters to reduce residual stress;
4) Inspect the straightness 100%;
5) Separate roughing and finishing;
6) Provide adequate cooling;
7) Keep the allowance uniform;
8) Include the machining distortion in the process.
GB/T 13342 Hydraulic Cylinders — Test Methods