E42-148 · Residual Stress Distortion · Welded Machine Frame · ★★
Insufficient annealing causes 0.05mm of springback when the residual stress releases after finish machining
[Insufficient Annealing] The annealing temperature and time were insufficient, so the welding residual stress did not relax fully.
[Springback] After finish machining removes the restraint the residual stress releases and the part springs back by 0.05mm.
[Design Omission] The annealing process did not meet the specification and the residual stress was not measured.
1) Set the annealing temperature and time according to the steel grade;
2) Calibrate the furnace temperature uniformity;
3) Measure the residual stress after annealing;
4) Age sufficiently before finish machining;
5) Measure the springback and compensate for it;
6) Sample the hardness for confirmation;
7) Optimise the furnace loading arrangement;
8) Include the annealing in the welding process.
JB/T 5000.3 Heavy Machinery — Welded Parts