Fretting Corrosion in an Interference Fit Causes Seizure

E43-171 · Interference Fit Failures · Water Pump Impeller ∅80, interference 0.04mm, after 2 years of service fretting corrosion seized it · ★★

Problem Symptom

The fretting wear produced oxides that rusted the mating surfaces together, and the part could not be removed during maintenance

Root Cause

[Mechanism] Microscopic sliding caused metal debris to oxidise and expand in volume, wedging into the mating surfaces and locking them together.
[Calculation] The fretting amount ε=δactual-δrequired=0.04-0.09=-0.05mm; long-term fretting built an oxide layer 0.1mm thick that locked the fit.
[Design Omission] Not enough interference was selected to prevent fretting and no rust protection was applied; this design flaw caused seizure.

Correct Solution

1) Raise the interference to 0.09~0.12mm;
2) Apply a rust-resistant coating;
3) Select stainless steel;
4) Rotate the part periodically;
5) Perform penetrant inspection;
6) Control the removal force;
7) Treat the surfaces;
8) Carry out a fretting test on the first piece.

Checklist

References

GB/T 5371-2004 Interference Fits — Calculation and Selection

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »