Press Fitting a Thin-Walled Bushing Causes Out-of-Round

E43-173 · Interference Fit Failures · Connecting Rod Bushing ∅45, thin wall 1.5mm, interference 0.05mm, out-of-round 0.03mm after pressing · ★★

Problem Symptom

The thin-walled bushing went out of round during pressing, giving an uneven bearing clearance that burned the bush

Root Cause

[Mechanism] Press fitting a thin-walled bushing with interference applies uneven pressure and causes plastic out-of-round.
[Calculation] The out-of-round amount e≈p·r³/(E·t²)=p×22.5³/(2.1e5×1.5²), with p=0.05×2.1e5/45=233MPa, gives e=0.031mm, which is out of specification.
[Design Omission] The coaxiality of the press fit was not controlled and no minimum bushing wall thickness was set; this design flaw caused out-of-round.

Correct Solution

1) Require a bushing wall thickness of ≥2mm;
2) Press on axis;
3) Reduce the interference to 0.03;
4) Select H7/m6;
5) Inspect the roundness;
6) Match and select parts by the measured bore and shaft sizes;
7) Grind and scrape to guarantee contact;
8) Measure the roundness on the first piece.

Checklist

References

GB/T 5371-2004 Interference Fits — Calculation and Selection