Knowledge Base › Tolerance and Fit Error Case › Motor Stator Lamination Accumulation

Motor Stator Lamination Accumulation

E43-487 · Dimensional-Chain Accumulation · Motor stator stack thickness designed 120±0.1, measured 122 after 50 laminations · ★★

Problem Description

Silicon-steel lamination stack accumulation made 2mm out of tolerance, shifting the magnetic circuit.

Root Cause

[Mechanism] Multi-lamination stack-thickness chain accumulated, so the closed loop (stack thickness) went out of tolerance.
[Calculation] T0=ΣTi=50×0.04=2, 20× the 0.1 allowance.
[Design Omission] No press-fit adjustment; design defect → stack thickness out of tolerance.

Corrective Solution

1) Provide a press-fit stop to absorb accumulation;
2) Match-machine each lamination per T0/√50;
3) Unify the datum;
4) Statistical check;
5) Selective matching by measurement;
6) Leave grinding stock;
7) Thickness gauge check;
8) First-article stack thickness measured ≤0.1.

Checklist

Reference

GB/T 755-2008 Rotating electrical machines — Rating and performance