Knowledge Base › Tolerance and Fit Error Case › Blade-to-Root Datum Misalignment

Blade-to-Root Datum Misalignment

E43-533 · Datum Misalignment · Blade located on the root while the design references the airfoil profile, causing a 0.5° twist overshoot · ★★

Problem Description

The blade-root datum does not coincide with the design airfoil profile, so the blade twist deviates by 0.5°.

Root Cause

[Mechanism] The blade-root datum does not coincide with the airfoil profile, so the root installation-angle error is carried into the twist.
[Calculation] The datum misalignment error is a 0.5° installation-angle offset, which is 2.5 times the twist allowance of 0.2°.
[Design Omission] The airfoil profile is not used as the datum; this design flaw leads to twist out-of-tolerance.

Corrective Solution

1) Use the airfoil profile as the locating datum;
2) Control the root installation angle;
3) Unify datum callouts;
4) Tolerance-allocate by datum offset;
5) Measure twist on the first article;
6) Note it in the process sheet;
7) Reduce datum transfers;
8) First-article twist measured ≤0.2°.

Checklist

Reference

GB/T 1182-2018 GPS — Geometrical tolerancing (form, orientation, location and run-out)