E43-327 · Thermal Deformation Uncompensated · A CNC machine guideway 3000mm long in cast iron, designed symmetric heating, measured one-sided 7℃ rise · ★★
Guideway temperature rise of 7℃ bent it, making straightness go 0.08mm out of tolerance and causing machining waviness.
[Mechanism] One-sided guideway heating bends it and the motion straightness deviates; tool marks show waviness.
[Calculation] α=10e-6, Δl=10e-6×3000×7=0.21mm; bending deflection ≈0.21/3=0.07mm out of tolerance.
[Design Omission] No symmetric thermal insulation or compensation — a design defect leading to straightness out of tolerance.
1) Add a symmetric insulation cover to the guideway to remove one-sided rise;
2) Add thermal compensation to correct the 0.07mm straightness;
3) Warm up before machining and re-measure the datum;
4) Symmetrically place drives to reduce torsion;
5) Monitor guideway temperature in real time and build compensation;
6) Select low-expansion cast iron to cut Δl;
7) Periodically re-measure straightness;
8) On first articles, measure straightness and verify ≤0.02mm.
GB/T 11336-2004 Straightness tolerances