E43-341 · Thermal Deformation Not Compensated · A roller shaft 800mm long, designed clearance, measured rise 70℃ striking the table · ★★
A 70℃ shaft temperature rise elongates the shaft by 0.64mm, making the roller strike the grinding table and causing abnormal noise.
[Mechanism] The roller shaft expands axially under heat; with insufficient cold-state clearance, the roller rim strikes the grinding table.
[Calculation] α=11.5e-6, Δl=11.5e-6×800×70=0.644mm≈0.64mm, exceeding the 0.5mm clearance and causing contact.
[Design Omission] No hot-state clearance was provided — a design defect leading to table contact.
1) Size the roller-rim clearance for hot elongation 0.64mm, ≥0.8mm;
2) Add cooling to the roller shaft to hold the rise ≤40℃;
3) Leave a floating end to compensate elongation;
4) Monitor axle temperature in real time with an alarm;
5) Use low-expansion shaft material to reduce Δl;
6) Re-check clearance periodically;
7) Run the first article to verify no rubbing;
8) Inspect for abnormal noise during operation.
JB/T 11108-2011 Vertical roller mills