Casting Mould Misalignment Causes Wall Thickness Deviation

E43-097 · Weld/Cast Forming Out of Tolerance · Housing Casting · ★★

Problem Symptom

A 0.40 mould misalignment made the wall thickness deviate by 2mm, and machining exposed sand holes

Root Cause

[Mould Misalignment] The upper and lower mould were offset by 0.40, so the wall thickness deviated.
[Exposed Sand] At the thin section machining exposed sand holes that leaked.
[Design Omission] Dowel pins should have been used for mould alignment with misalignment inspected, but misalignment was not controlled.

Correct Solution

1) Use dowel pins for mould alignment;
2) Keep misalignment ≤0.20;
3) Keep the wall thickness even;
4) Qualify the casting process;
5) Perform NDT after rough machining;
6) Section the first piece;
7) Leave adequate machining allowance;
8) Scrap and re-cast out-of-specification parts.

Checklist

References

GB/T 9439-2010 Grey Iron Castings