Gear Blank Casting Distortion Causing Blank Runout Error

E43-363 · Welded/Cast Forming Dimensional Error · A gear blank 300mm diameter, designed blank radial runout 0.03, measured casting distortion 0.12 · ★★

Problem Description

Casting distortion of the gear blank pushes radial runout 0.12mm out of tolerance, leaving the tooth ring eccentric after hobbing.

Root Cause

[Mechanism] Uneven cooling deforms the casting, offsetting the datum outer circle; after hobbing the tooth ring runs radially off.
[Calculation] Radial runout≈2e=2×0.06=0.12mm (e is eccentricity), 4× the tolerance of 0.03.
[Design Omission] No rough-turning datum or aging — a design defect leading to runout error.

Corrective Solution

1) After casting, rough-turn the datum outer circle and align it;
2) Age before rough turning to relieve stress;
3) Establish a center-hole datum;
4) Finish-turn the blank to hold runout;
5) Measure radial runout with a dial indicator;
6) Provide evenly distributed process pads;
7) Improve casting accuracy;
8) Measure first-article runout ≤0.03mm.

Checklist

Reference

GB/T 10095.1-2008 Cylindrical gears — Accuracy system — Part 1