E44-234 · Pump Selection & Cavitation · Grey Cast Iron Impeller Centrifugal Pump IS100-80-160 · ★★
The impeller was HT200 grey cast iron and slight cavitation pitted it 2mm deep within half a year, roughening the flow passage and reducing the efficiency
[Cavitation] The material has poor cavitation resistance, so even slight cavitation produces rapid pitting and spalling.
[Calculation] Grey cast iron is far less resistant to cavitation than stainless steel, and the bubble collapse impact, which can reach the MPa level, makes the brittle cast iron spall quickly.
[Design Omission] A cast iron impeller was still used in a cavitation-prone duty and the material was not selected for cavitation resistance, so pitting occurred.
1) Change the impeller to a cavitation-resistant material such as duplex steel or aluminium bronze: a tough material resists the collapse impact, so the pitting is delayed;
2) Remove the cavitation source at the root by raising NPSHa: with no cavitation there is no pitting, so this treats the cause;
3) Apply an erosion-resistant coating to the flow passage: the coating resists the impact, so the base material is protected;
4) Optimise the leading-edge profile to reduce the local low pressure: a good profile raises the local pressure, so there is less cavitation;
5) Inspect the impeller for pitting at regular intervals: the damage progresses gradually, so the impeller is replaced in time;
6) Control the operation so the pump runs in the high-efficiency region with minimal off-design running: off-design running cavitates, so the damage is reduced;
7) Commission the pump and observe it in service for abnormal pitting: the design requirement must be verified by measurement, so this confirms the delivery;
8) Include the cavitation-resistant material selection in the design: the original choice of cast iron was the root cause, so the design must always include it.
GB/T 13006-2013 Centrifugal Pumps - NPSH