Slurry abrasion combined with cavitation destroys the impeller

E44-243 · Pump Selection & Cavitation · Slurry pump 100ZJ-I-A42 · ★★★

Problem Symptom

The medium contained 30% solids; abrasion in the mild cavitation zone acted synergistically with cavitation, the impeller inlet was worn through within half a year and the flow fell by 20%

Root Cause

[Cavitation] A solids-laden slurry suffers abrasion in the cavitation zone that acts synergistically with cavitation, and the combined destruction rate far exceeds either mechanism alone.
[Calculation] The impact of collapsing vapour bubbles superimposes on the scouring of solid particles, and the synergistic wear rate is about 2 to 3 times the pure abrasion rate, which wore through the impeller in half a year.
[Design Omission] The slurry duty was not de-cavitated and no wear-resistant material was selected, so the synergistic destruction occurred.

Correct Solution

1) Eliminate the cavitation source as the first priority (raise NPSHa), because cavitation amplifies abrasion, thereby breaking the synergy;
2) Select a high-chromium wear-resistant alloy or a rubber lining for the impeller, because wear-resistant material resists particle scouring, thereby extending life;
3) Reduce the impeller peripheral speed to limit abrasion, because wear rate scales with v³, thereby slowing the wear;
4) Keep the solids content within the design range, because exceeding it aggravates the wear, thereby controlling the solids content;
5) Apply a wear-resistant coating to the flow-path parts, because the coating resists scouring, thereby protecting them;
6) Inspect the wear trend at regular intervals, because the wear is progressive, thereby allowing timely replacement;
7) Measure during commissioning to confirm there is no cavitation and that the wear rate meets the target, because the design requirement must be verified by measurement, thereby closing out the acceptance;
8) Incorporate slurry-specific abrasion and cavitation design into the selection, because the absence of a dedicated slurry design was the root cause, so the design must include it.

Checklist

References

GB/T 13006-2013 Centrifugal Pumps - NPSH