E44-971 · Vessel Strength and Wall-Thickness Deficiency · Pressure vessel · ★★★
Low factor, weakness, hazard
[Mechanism] The yield/tensile safety factor was taken below the GB/T 150 requirement, inflating the allowable stress and thinning the wall; internal pressure then pushed the actual stress beyond allowable and lost strength.
[Calculation] Rm=410MPa, n taken as 2.4 (needs ≥3.0); [σ]=410/2.4=171MPa (should be 137MPa). Required δ=PCK/(2[σ]φ-P): 7.2mm at 171, 9.0mm at 137 — short by 1.8mm.
[Design Omission] No safety-factor check, no prescribed n, and no wall recalculation.
1) Recalculate per GB/T 150 with n≥3.0 (was 2.4), dropping [σ] to 137MPa and requiring δ 9.0mm, since low n thinned the wall and adding thickness lowers stress — thus restoring strength;
2) Check that the material strength limit Rm matches n, since a low strength grade weakens the vessel and a strength check assures it — thus compliant strength;
3) Thicken the wall to 9.0mm (was 7.2mm), since a thin wall loses strength and a thicker one raises it — thus reinforcing;
4) Upgrade the material grade (Q345R for Q235B), since a low grade weakens the vessel and a higher grade raises the allowable — thus raising strength;
5) Perform ultrasonic thickness measurement (every point ≥9mm), since thinning first shows as wall loss and can be replaced early — thus monitoring thickness;
6) Run a hydrotest (1.25×1.6=2.0MPa held), since n was never checked and measurement confirms no leak — thus setting strength by data;
7) In operation, hold pressure ≤1.6MPa (reduce if exceeded), since exceeding n raises stress and pressure control prevents deformation — thus running to prevent weakening;
8) Write the factor and strength check into the calculation book, since the inadequate-factor root cause was the missed n check and missing wall recalc — thus locking it in at design.
GB/T 150.1-2011 Pressure vessels