E44-973 · Vessel Strength and Wall-Thickness Deficiency · Pressure vessel · ★★★
Bulge, protrusion, deformation
[Mechanism] A local region buckles outward under external pressure or added load, the hoop stress exceeding the critical buckling stress.
[Calculation] Local σ=185MPa exceeds the 150MPa critical buckling stress; the bulge is 12mm high, 80mm diameter, on a 6mm wall — under-stable.
[Design Omission] No local-stability check, no stiffening rings, and no bulge inspection.
1) Check local stability (hold σ≤0.8σcr=120MPa), since σ>150MPa causes bulging and the stability check lowers it — thus preventing bulge;
2) Add external stiffening rings (channel [14 at 800mm spacing), since a weak shell bulges and rings raise stiffness — thus stabilizing shape;
3) Raise the wall to 9mm (was 6mm), since a thin wall bulges and a thicker one raises stability — thus reinforcing;
4) Switch to high-strength steel (Q345R for Q235B), since a soft shell bulges and stronger steel raises stiffness — thus stiffening;
5) Perform ultrasonic bulge measurement (every point ≤3mm high), since a bulge first shows as a protrusion and can be replaced early — thus checking bulge;
6) Run an external-pressure stability test (0.1MPa held), since the bulge came from an unvalidated design and measurement confirms stability — thus setting stability by data;
7) Hold external pressure ≤0.05MPa (vent if exceeded), since over-stable pressure bulges and pressure control prevents it — thus running to prevent bulge;
8) Write the stability check and ring addition into the calculation book, since the bulge root cause was the missed local-stability check and missing rings — thus locking it in at design.
GB/T 150.1-2011 Pressure vessels