E44-974 · Vessel Strength and Wall-Thickness Deficiency · Support · ★★★
Large reaction, cracking, deformation
[Mechanism] The saddle reaction exceeded the shell's local load capacity and was unevenly distributed, producing high local stress in the wall above the saddle and cracking it.
[Calculation] Saddle reaction R=320kN, wrap angle 120°, local σ=240MPa exceeds [σ]=185MPa; no wear pad was fitted, concentrating the stress.
[Design Omission] No support-reaction check, no load equalization, and no wear pad.
1) Check the saddle reaction (hold R≤ design capacity and σ≤185MPa), since R=320kN gave σ=240MPa and cracking, and checking the force lowers it — thus preventing cracking;
2) Equalize the load on the two saddles (spread ≤5%), since an uneven load cracks and equal load levels it — thus balancing load;
3) Add saddle wear pads (δ=10mm, fitted flush and fully welded), since no pad concentrated stress and a pad spreads it — thus lowering stress;
4) Raise foundation capacity (widen the C25 concrete), since a weak foundation cracks and a stronger one stabilizes — thus stabilizing the support;
5) Ultrasonic-test the support zone (no cracks at any point), since cracks first show as lines and can be rejected early — thus finding cracks;
6) Run a water-filling test (1.0× liquid level held), since the crack came from an unvalidated design and measurement confirms stability — thus setting capacity by data;
7) Hold the fill rate ≤2m/h (fast filling biases the load), since a fast rise induces bias and a slow one equalizes — thus filling smoothly;
8) Write the reaction check and load equalization into the calculation book, since the cracking root cause was the missed R check and uneven load — thus locking it in at design.
GB/T 150.1-2011 Pressure vessels