E44-990 · Vessel Strength and Wall-Thickness Deficiency · Support · ★★★
Pad not seated, cracking, deformation
[Mechanism] A gap existed between the saddle wear pad and shell, locally losing contact; stress concentration went beyond allowable and cracked.
[Calculation] Gap 3mm, local σ=220MPa exceeds [σ]=185MPa, contact area only 40%, stress concentration factor 2.2×.
[Design Omission] The pad was not seated, no fit check, and no NDE.
1) Seat and fully weld the pad to the shell (gap ≤0.5mm), since a loose pad concentrates stress and a seated one spreads it — thus lowering stress;
2) Check fit (feeler gauge gap ≤0.5mm all around), since a loose pad cracks and a fitted one bonds — thus seating it;
3) Fully weld the pad (continuous weld, no cold lapping), since hollow cold welds crack and a full weld is solid — thus seating firmly;
4) Raise the pad to 12mm thick (was 8mm), since a thin pad cracks and a thick one raises strength — thus reinforcing;
5) Perform MT on the pad zone (no cracks), since cracks first show as lines and can be rejected early — thus finding cracks;
6) Run a hydrotest (1.25× design pressure), since the unseated pad caused cracking and measurement confirms stability — thus setting strength by data;
7) Control assembly gap (level during final assembly), since bias separates and leveling seats — thus assembling to fit;
8) Write the seating and fit check into the assembly card, since the pad-not-seated root cause was the missed seating and unchecked fit — thus locking it in at assembly.
GB/T 150.1-2011 Pressure vessels