E44-991 · Vessel Strength and Wall-Thickness Deficiency · Head · ★★★
Straight-flange crack, leak, fracture
[Mechanism] The joint between the head straight-flange and the shell concentrates forming/welding stress; an overly short straight flange cracks.
[Calculation] Straight-flange height h=25mm too short, transition R=15mm less than 3δ=30mm, local σ=210MPa exceeds [σ].
[Design Omission] No transition-radius check, no straight-flange check, and no NDE.
1) Switch to a smooth transition (R≥3δ=30mm), since a sharp corner cracks and a transition lowers stress — thus lowering stress;
2) Check the straight-flange height and transition radius (h to standard, R≥30mm), since a small radius cracks and the check sets it right — thus compliant;
3) Add local reinforcement (butter the transition zone), since a weak zone cracks and reinforcement raises strength — thus reinforcing;
4) Switch to a tougher material (normalized 16MnDR); brittle material cracks, a tougher material resists cracking;
5) Perform MT on the straight-flange zone (no cracks), since cracks first show as lines and can be rejected early — thus finding cracks;
6) Run a hydrotest (1.25× design pressure), since the transition crack was untested and measurement confirms stability — thus setting strength by data;
7) Control the welding sequence (symmetrical to prevent distortion); uncontrolled welding introduces stress, a sequenced weld balances it;
8) Write the transition-radius check into the calculation book, since the straight-flange crack root cause was the too-small R and missed check — thus locking it in at design.
GB/T 150.1-2011 Pressure vessels