E44-198 · Other · Flange Bonding Terminal · ★★★
The bonding terminal corroded and broke; static could not be conducted away, creating a spark hazard.
[Corrosion Break] The terminal corroded and broke the bond.
[Spark] Static voltage exceeding the limit discharges.
[Design Omission] No corrosion protection and no inspection; a hazard remained.
1) Choose stainless or plated bonding terminals for corrosion resistance; corrosion breaks the bond and creates a static spark hazard, so protect against corrosion to keep continuity;
2) Sleeve the bonding wire against corrosion; exposed wire corrodes, so sleeve it;
3) Periodically measure bonding continuity; it breaks gradually, so test periodically;
4) Hold the grounding-grid resistance ≤10Ω; high resistance does not discharge, so control resistance;
5) Design for explosion-proofing in flammable areas; sparks ignite, so make it explosion-proof;
6) Add a static alarm that trips on a broken bond; a break is hard to notice, so alarm it;
7) Verify jumper continuity and absence of spark on commissioning; design requirements need measured confirmation, so confirm at delivery;
8) Bring corrosion inspection into anti-static design; the original lack of inspection was the root cause of the corrosion break, so the design must include it.
GB 12158-2006 General guide for preventing static electricity accidents