E44-329 · Excessive Piping Resistance and Pressure Drop · Process Pipe with Left-Over Electrode/Rag · ★★
A left-over welding electrode in the pipe blocked 30% of the section, raised local v, Δp=0.1MPa, and cut downstream flow 25%.
[Blockage] Debris occupies the section, shrinking flow area and spiking v.
[Flow Drop] Δp=0.1 cuts downstream flow 25%.
[Design Omission] No pigging and air purge, and no diameter-through test; debris blocked it.
1) Pig and air-purge before commissioning; a left-over electrode blocked 30%, Δp=0.1, flow dropped 25%, so clear debris;
2) Run a diameter-through test to confirm full flow; hidden blockage is hard to notice, so verify it;
3) Cap openings during installation to prevent debris from falling in; open ends easily admit debris, so cap them;
4) Fit a Y-strainer to catch debris; residual debris re-blocks, so trap it;
5) Add downstream flow monitoring to catch the drop early; a blockage lowers flow, so monitor it;
6) Add a temporary strainer at the pump inlet; debris damages the pump, so temporary-filter it;
7) Periodically disassemble and inspect high-risk sections; blind sections accumulate, so open and inspect;
8) Bring purging into commissioning; the original lack of purge was the root cause of blockage, so commissioning must gate it.
GB/T 20801.3-2020 Design code for industrial metallic piping