E44-334 · Excessive Piping Resistance and Pressure Drop · Aged carbon-steel pipe covered in rust pits · ★★
Rust pitting raises equivalent roughness ε=1.5mm and λ=0.045 (above a new pipe's 0.02), doubling hf
[Mechanism] Rust pitting raises ε to 1.5mm and λ to 0.045.
[Calculation] The doubled λ doubles hf.
[Design Omission] No internal corrosion protection and no pipe replacement - rust roughness kept resistance high.
1) Sand-blast the interior and apply epoxy lining, since ε=1.5 drove λ=0.045 and doubled hf, cutting roughness and λ;
2) Replace badly corroded sections with stainless or plastic-lined pipe, since rust cannot be restored, replacing the pipe;
3) Compute λ from the real ε using Colebrook, since a fictitious λ understates loss, using a correct λ;
4) Periodically inspect rust by bore camera, since rust creeps unnoticed, inspecting rust;
5) Control medium corrosivity, since corrosion causes roughness, controlling corrosion;
6) Compute hf with the real λ and margin, since raised resistance lowers the end pressure, leaving margin;
7) Boost pump head to cover the added resistance, since the end needs pressure, adding head;
8) Include internal corrosion protection in maintenance, since the missing protection was the root cause, closing the loop at maintenance.
GB/T 20801.3-2020 Design code for industrial metallic piping